Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |