Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 25.1 J @Thickness 1.85 mm, Temperature 23.0 °C |
18.5 ft-lb @Thickness 0.0728 in, Temperature 73.4 °F |
ductile, 3.30 m/sec; ASTM D3763 |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |