Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 9.99 - 23.5 J @Temperature -20.0 - -20.0 °C |
7.37 - 17.3 ft-lb @Temperature -4.00 - -4.00 °F |
Average value: 16.7 J Grade Count:1 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Dart Drop, Total Energy | 9.99 - 23.5 J @Thickness 3.18 - 3.18 mm |
7.37 - 17.3 ft-lb @Thickness 0.125 - 0.125 in |
Average value: 16.7 J Grade Count:1 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |