Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 19.8 - 21.9 J @Temperature -18.0 - 0.000 °C |
14.6 - 16.2 ft-lb @Temperature -0.400 - 32.0 °F |
Average value: 20.8 J Grade Count:1 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dart Drop, Total Energy | 19.8 - 21.9 J @Thickness 1.85 - 1.85 mm |
14.6 - 16.2 ft-lb @Thickness 0.0728 - 0.0728 in |
Average value: 20.8 J Grade Count:1 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dart Drop, Total Energy | 19.8 J @Thickness 1.85 mm, Temperature -18.0 °C |
14.6 ft-lb @Thickness 0.0728 in, Temperature -0.400 °F |
brittle, 3.30 m/sec; ASTM D3763 |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |