Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 8.30 MPa @Temperature 870 °C, Time 3.60e+6 sec |
1200 psi @Temperature 1600 °F, Time 1000 hour |
Typical Stress-Rupture |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |