Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 475 MPa @Temperature 704 °C, Time 3.60e+6 sec |
68900 psi @Temperature 1300 °F, Time 1000 hour |
|
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |