Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 620 MPa @Temperature 732 °C, Time 324000 sec |
89900 psi @Temperature 1350 °F, Time 90.0 hour |
|
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur.. |
|||
Rupture Strength | 620 MPa @Temperature 760 °C, Time 36000 sec |
89900 psi @Temperature 1400 °F, Time 10.0 hour |
|
Crucible Compaction Metals Rene 95 Nickel Based Superalloy P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and.. |
|||
Rupture Strength | 620 MPa @Temperature 760 °C, Time 198000 sec |
89900 psi @Temperature 1400 °F, Time 55.0 hour |
|
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained.. |