Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 6.89 MPa @Temperature 982 °C, Time 1.08e+8 sec |
999 psi @Temperature 1800 °F, Time 30000 hour |
|
Carlson C 800H Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists.. |