Mechanical Properties Metric English Comments
Rupture Strength 32.0 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
4640 psi

@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 34Ni/25Cr/Nb No. HR 33 Nb
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Rupture Strength 32.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
4640 psi

@Temperature 1560 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 37Ni/18Cr No. HR5
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..