Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 27.0 MPa @Temperature 800 °C, Time 3.60e+7 sec |
3920 psi @Temperature 1470 °F, Time 10000 hour |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Rupture Strength | 27.0 MPa @Temperature 750 °C, Time 3.60e+7 sec |
3920 psi @Temperature 1380 °F, Time 10000 hour |
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |