Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rupture Strength = 3770 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 26.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
3770 psi

@Temperature 1380 °F,
Time 10000 hour
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Rupture Strength 26.0 MPa

@Temperature 815 °C,
Time 360000 sec
3770 psi

@Temperature 1500 °F,
Time 100 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Rupture Strength 26.0 MPa

@Temperature 760 °C,
Time 3.60e+6 sec
3770 psi

@Temperature 1400 °F,
Time 1000 hour
Typical Stress-Rupture
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Copyright © lookpolymers.com All Rights Reserved