Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 206 MPa @Temperature 550 °C, Time 3.60e+7 sec |
29900 psi @Temperature 1020 °F, Time 10000 hour |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |