Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 219 MPa @Temperature 871 °C, Time 3.60e+6 sec |
31800 psi @Temperature 1600 °F, Time 1000 hour |
|
Special Metals UDIMET® alloy 720 Nickel Base Alloy UDIMET® alloy 720 is a nickel base alloy, solid solution strengthened with tungsten and molybdenum and precipitation-hardened with titanium and aluminum. The alloy combines high strength with me.. |