Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 145 MPa

@Temperature 816 °C,
Time 3.60e+6 sec
21000 psi

@Temperature 1500 °F,
Time 1000 hour
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy
UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm..