Rupture Strength 9.70 MPa

@Temperature 1095 °C,
Time 3.60e+6 sec
1410 psi

@Temperature 2003 °F,
Time 1000 hour
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..