Mechanical Properties Metric English Comments
Rupture Strength 7.00 MPa

@Temperature 1000 °C,
Time 3.60e+7 sec
1020 psi

@Temperature 1830 °F,
Time 10000 hour
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Rupture Strength 7.00 MPa

@Temperature 1050 °C,
Time 3.60e+7 sec
1020 psi

@Temperature 1920 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 37Ni/18Cr No. HR5
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..