Polymer Property : Hardness, H358/30 = 84.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 84.0 MPa
12200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East)
XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa..