Mechanical Properties Metric English Comments
Hardness, H358/30 82.0 MPa
11900 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® CL101 PBT+PC
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Hardness, H358/30 82.0 MPa
11900 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Hardness, H358/30 82.0 MPa
11900 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..