Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 101 - 234 MPa | 14600 - 33900 psi | Average value: 142 MPa Grade Count:10 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |