Polymer Property : Hardness, H358/30 = 26800 psi
Polymer Property :
Hardness, H358/30 =
26800 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Hardness, H358/30
185
MPa
26800
psi
ISO 2039-1
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East)
20% GF Super High Flow PBT