Mechanical Properties Metric English Comments
Hardness, H358/30 121 MPa
17500 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
Hardness, H358/30 121 MPa
17500 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific)
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
Hardness, H358/30 121 MPa
17500 psi
ISO 2039-1
Eurostar Staramide B40 PA6, Extrusion
Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar.