Polymer Property : Hardness, H358/30 = 16500 psi
Polymer Property :
Hardness, H358/30 =
16500 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Hardness, H358/30
114
MPa
16500
psi
ISO 2039-1
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East)
10% GF FR PBT/PC Blend