Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 104 MPa | 15100 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Hardness, H358/30 | 104 MPa | 15100 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
Hardness, H358/30 | 104 MPa | 15100 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
Hardness, H358/30 | 104 MPa | 15100 psi | ISO 2039-1 |
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East) GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req.. |