Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 103 MPa | 14900 psi | ISO 2039-1 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR2210 compound is based on an aternative polymeric wear technology and does not contain silicones. LEXAN WR2210 has superior processability (flow similar to LEXAN 121) and par.. |
|||
Hardness, H358/30 | 103 MPa | 14900 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |