Mechanical Properties Metric English Comments
Hardness, H358/30 109 MPa
15800 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East)
XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli..