Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0222 GPa | 3.22 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |