Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |