Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0110 GPa | 1.60 ksi | ISO 37 |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
50% Modulus | 0.0110 GPa | 1.60 ksi | |
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth.. |