Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00634 GPa | 0.920 ksi | |
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re.. |