Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00580 GPa | 0.841 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
50% Modulus | 0.00580 GPa | 0.841 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060EM PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |