Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00150 GPa | 0.218 ksi | ASTM D412 |
Network Polymers Softflex® 2701 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
50% Modulus | 0.00150 GPa | 0.218 ksi | ASTM D412 |
Network Polymers Softflex® 2701T Transparent Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
50% Modulus | 0.00150 GPa | 0.218 ksi | ASTM D412 |
Network Polymers Softflex® 2910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
50% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
50% Modulus | 0.00150 GPa | 0.218 ksi | DIN 53504 |
Lubrizol ESTANE® 54660 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |