Polymer Property : 50% Modulus = 0.174 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.00120 GPa
0.174 ksi
Conductive CR Conveyor Belt Cover Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
50% Modulus 0.00120 - 0.00140 GPa
0.174 - 0.203 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..