Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.000600 - 0.00100 GPa
0.0870 - 0.145 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 80 Silicone TPE
SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
50% Modulus 0.000600 - 0.00100 GPa
0.0870 - 0.145 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..