Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0275 GPa | 3.99 ksi | ASMT D638 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
50% Modulus | 0.0275 GPa | 3.99 ksi | ASTM D638 |
Toyobo PELPRENE™ S6002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |