Mechanical Properties Metric English Comments
50% Modulus 0.0235 GPa
3.41 ksi
ISO 37
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..