Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0172 GPa | 2.49 ksi | ASTM D412 |
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |