Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0153 GPa | 2.22 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR5725 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
50% Modulus | 0.0153 GPa | 2.22 ksi | ASTM D412 |
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in.. |