Mechanical Properties Metric English Comments
50% Modulus 0.0116 GPa
1.68 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..