Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00903 GPa | 1.31 ksi | 10 in/min; ASTM D412 |
PolyOne Elastamax XL-0257-1 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |