Polymer Property : 50% Modulus = 0.00820 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.00820 GPa
1.19 ksi
ISO 37
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00820 GPa
1.19 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
50% Modulus 0.00820 GPa
1.19 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR5020 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..