Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00690 GPa | 1.00 ksi | ASTM D412 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
50% Modulus | 0.00690 GPa | 1.00 ksi | |
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-45D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane.. |