Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00610 GPa | 0.885 ksi | ISO 37 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |