Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00414 GPa | 0.600 ksi | ASTM D412 |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |