Polymer Property : Tensile Creep Modulus, 1000 hours = 9000 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 9000 MPa
1.31e+6 psi
ISO 899-1
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..