Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 600 MPa @Temperature 23.0 °C |
87000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 600 MPa | 87000 psi | ISO 899-1 |
Lanxess Durethan® B 30 S 000000 Nylon 6 PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification |
|||
Tensile Creep Modulus, 1000 hours | 600 MPa @Time 3.60e+6 sec |
87000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D.. |