Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 21.7457 - 83.3376 MPa @Temperature 40.0 - 100 °C |
3153.95 - 12087.1 psi @Temperature 104 - 212 °F |
Average value: 49.2 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Creep Modulus, 1000 hours | 21.7457 - 83.3376 MPa @Pressure 0.500 - 7.00 MPa |
3153.95 - 12087.1 psi @Pressure 72.5 - 1020 psi |
Average value: 49.2 MPa Grade Count:1 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |