Polymer Property : Tensile Creep Modulus, 1000 hours = 696000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4800 MPa
696000 psi
Covestro Makrolon® 8025 Polycarbonate
High viscosity extrusion and injection molding grade with 20% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b..
Tensile Creep Modulus, 1000 hours 4800 MPa

@Time 3.60e+6 sec
696000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra..