Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4500 MPa
653000 psi
ISO 899-1
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 4500 MPa
653000 psi
ISO 899-1
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 4500 MPa
653000 psi
ISO 899-1
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Creep Modulus, 1000 hours 4500 MPa
653000 psi
ISO 899-1
BASF Ultraform® N2200 G43 POM
Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF
Tensile Creep Modulus, 1000 hours 4500 - 12000 MPa
653000 - 1.74e+6 psi
Average value: 7400 MPa Grade Count:10
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Tensile Creep Modulus, 1000 hours 4500 MPa

@Strain <=0.500 %
653000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT
Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs..