Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4320 MPa
627000 psi
At 1% Deformation; DIN 53444
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..