Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 230 MPa
33400 psi
23°C; ISO 899; DIN 53444
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH
Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased...